| Home | Product | Order | Contact Us |
Organic Pigments
Inorganic Pigments
Fluorescent Pigments
Pearlescent Pigments
Aluminum Oxide (Al2O3)
Silicon Oxide (SiO2)
Titanium Oxide (TiO2)
Zinc Oxide (ZnO)
Yttrium Oxide (Y2O3)
Zirconium Oxide (ZrO2)
Cerium Oxide (CeO2)
Large Surface Area Al2O3
Large Surface Area CeO2
Rare Earth-Zr Complex Oxide
Alumina Supported Rare Earth-Zr Complex Oxide
Rare Earth-Zr Complex Carrier Coating
Cerium Oxide (CeO2)
Aluminum Oxide (Al2O3)
Zirconium Oxide (ZrO2)
Chromium Oxide (Cr2O3)
Long Persistence Phosphors
UV Phosphors
IR Phosphors
Antibacterial Powder
Conductive Powder
Anti-Ultraviolet Powder
Far-Infrared Ceramic Powder
Ion Powder
Photocatalyst Powder
Others

 

Rare Earth −Zr Complex Carrier Coating

[Applied Field]

  • Catalyst for cleaning exhaust gases of automotives and motorcycles

  • Cleaning of industrial organic exhaust gases and indoor air

  • Catalyst for nature gases combustion

  • Catalytic decomposition in fluidized-bed in oil refining industry

[Product Properties]

  • Using different forms of rare earth, Zr and Al compounds as raw materials, the coatings after baking will have the best oxygen storage and release capability and specific surface area stability.

  • Through fully rubbing and precise classification, the coarse particles in the powder can be wiped off. Therefore, it will achieve uniform distribution of the rare-earth and alumina particles, which can avoid sedimentation while using and the coating thickness can be controlled more easily.

  • Doped with nano Al2O3 and CeO2, the bonding stress of coatings will increase, which can avoid chapping and peeling while using and give the carrier strong resistance to the wet hot current erosion.

[Technology Parameters]

Model

RC−25AS

RC−35AS

Appearance

yellowish

yellowish

Main Composition

(La0.05Y0.05
Ce0.6Zr0.3)O2, γ-Al2O3

(La0.05Y0.05
Ce0.3Zr0.6)O2 ,γ-Al2O3

Solid content

40 ± 2 %

40 ± 2 %

D50

1.0-1.5 μm

1.0-1.5 μm

Fresh Specific Surface Area

150 -250 m2 /g

150 -250 m2 /g

Aging Specific Surface Area
(1000ºC 4hr m2/g)

40 − 60 m2 /g

50 − 70 m2 /g

[Instruction]

  • Swill out the product and mix, estimate the concentration according to the coating dosage and adjust to PH=2~3 with nitric acid

  • Reinforce water according the absorption of the carrier during coating and mix to assure stable solid content

  • The content of the transition elements such as Mn2+,Co3+ and the solid can be adjusted according to the request of users.

-------Asking for detailed materials and Samples-------

   

© 2007−2010 DBChemic, All Rights Reserved
Email: info@dbchemic.com
Tel:909-859-9052 Fax:775-551-9052
Address: 1926 W Holt Ave, Pomona, CA, 91768